Alloy
|
%
|
Ni
|
Cr
|
Fe
|
C
|
Mn
|
Si
|
Cu
|
S
|
Al
|
Ti
|
800
|
Min. |
30
|
19
|
|
|
|
|
|
|
0.15
|
0.15
|
Max.
|
35
|
23
|
balance
|
0.10
|
1.5
|
1
|
0.75
|
0.015
|
0.60
|
0.60
|
|
800H
|
Min.
|
30
|
19
|
|
0.05
|
|
|
|
|
0.15
|
0.15
|
Max.
|
35
|
23
|
balance
|
0.10
|
1.5
|
1
|
0.75
|
0.015
|
0.60
|
0.60
|
|
800HT
|
Min.
|
30
|
19
|
|
0.06
|
|
|
|
|
0.15
|
0.15
|
Max.
|
35
|
23
|
balance
|
0.10
|
1.5
|
1
|
0.75
|
0.015
|
0.60
|
0.60
|
|
AI+Ti: 0.85-1.20
|
Density
|
8.0 g/cm³
|
Melting point
|
1350-1400°C
|
Alloy
|
Tensile strength
Rm N/mm² |
Yield strength
R P 0. 2N/mm² |
Elongation
A 5 % |
800
|
500
|
210
|
35
|
800H
|
450
|
180
|
35
|